API 650 - Section - 9 (WELDING PROCEDURE AND WELDER QUALIFICATIONS) Flashcards

(12 cards)

1
Q

Welding procedures for ladder and platform assemblies,
handrails, stairways, and other miscellaneous assemblies, but not their attachments to the tank, shall comply with either ,,,,,

A

AWS D1.1, AWS D1.6, or Section IX of the ASME Code

How well did you know this?
1
Not at all
2
3
4
5
Perfectly
2
Q

Material with strength < 485 MPa (70 ksi)—

A

Group 1;

How well did you know this?
1
Not at all
2
3
4
5
Perfectly
3
Q

Material with strength ≥ 485 MPa (70 ksi) but < 550 MPa (80 ksi)—

A

Group 2

How well did you know this?
1
Not at all
2
3
4
5
Perfectly
4
Q

Material with strength ≥ 550 MPa (80 ksi)—

A

Group 3

How well did you know this?
1
Not at all
2
3
4
5
Perfectly
5
Q

Separate welding procedures and performance qualifications shall be conducted for,,,,,,,,,,,,

A

A841M/A841 material

How well did you know this?
1
Not at all
2
3
4
5
Perfectly
6
Q

For all materials to be used at a design metal temperature below ,,,,,,,,,,, the qualification of the
welding procedure for vertical joints shall include impact tests of the weld metal

A

10 °C (50 °F), (for vertical joint & Welding procedure)

How well did you know this?
1
Not at all
2
3
4
5
Perfectly
7
Q

If vertical joints are to be made by a

machine, automatic, or semiautomatic process, impact tests of the ,,,,,,,,,,, shall also be made

A

heat-affected zone

How well did you know this?
1
Not at all
2
3
4
5
Perfectly
8
Q

When the design metal temperature is below,,,,,,,,,,,,,,,,impact tests of the weld metal shall be made for all procedures used for welding the components

A

–7 °C (20 °F), (for All Welds & Procedures)

How well did you know this?
1
Not at all
2
3
4
5
Perfectly
9
Q

Impact tests shall show minimum values for …….

for P-No. 1, Group 1, materials………
for P-No. 1, Group 2, materials……..
for P-No. 1, Group 3, materials……….

A
20 J (15 ft-lbf)
27 J (20 ft-lbf)
34 J (25 ft-lbf)
How well did you know this?
1
Not at all
2
3
4
5
Perfectly
10
Q

For shell plates thicker than ,,,,,,, these values shall be increased by ,,,,,,,,,,,,,, for each ,,,,,,, over 40 mm (11/2 in.). Interpolation is permitted

A
40 mm (11/2 in.)
7 J (5 ft-lbf)
13 mm (1/2 in.)
How well did you know this?
1
Not at all
2
3
4
5
Perfectly
11
Q

Weld-metal impact specimens shall be taken across the weld with one face substantially parallel to and
within ,,,,,,,,,,,,,of the surface of the material.

A

1.5 mm (1/16 in.)

How well did you know this?
1
Not at all
2
3
4
5
Perfectly
12
Q

The welder or welding operator’s identification mark shall be hand- or machine-stamped adjacent to and at intervals not exceeding ,,,,,,,along the completed welds.

A

1 m (3 ft)

How well did you know this?
1
Not at all
2
3
4
5
Perfectly