Welding Procedure and Welder Qualification Flashcards

(3 cards)

1
Q

Who is normally responsible for the qualification of welding procedures and welders?

a. welder
b. architect
c. welder’s employer
d. independent test lab
e. code body

A

c. welders employer

How well did you know this?
1
Not at all
2
3
4
5
Perfectly
2
Q

What is the pipe welding position in which the pipe remains fixed with its axis horizontal, and the welder must weld around the joint?

a. 1G
b. 2G
c. 5G
d. 6G
e. 6GR

A

c. 5G

How well did you know this?
1
Not at all
2
3
4
5
Perfectly
3
Q

What is the necessary pipe position test for welders who are trying to qualify to weld T-, Y-, and K- connections?

a. 1G
b. 2G
c. 5G
d. 6G
e. none of the above

A

d. 6G

How well did you know this?
1
Not at all
2
3
4
5
Perfectly